Channel Industries 5700 Lead Zirconate Titanate Piezoelectric

 

Subcategory: Oxide, Other; Oxide, Zirconium; Piezoelectric; Oxide

Key Words: PZT; Lead Zirconium Titanium Oxide

Material Notes:
Navy Type VI

Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used material for electro-mechanical and electro-acoustic transducers.

Uses of this grade include: Hydrophones; Shallow; Vibration Pickups; Accelerometers; Receiver Transducers; High Static Motion Transducers; Non-Destructive Testing; Audible Alarms

Data provided by Channel Industries, Inc.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Curie Temperature
  • Dielectric Constant
  • Dissipation Factor
  • Piezoelectric Longitudinal Coupling Factor, k33
  • Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V
  • Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V
  • Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N
  • Piezoelectric Planar Coupling Factor, kp
  • Piezoelectric Mechanical Q
  • Piezoelectric Shear Coupling Factor, k15
  • Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V
  • Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N
  • Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N
  • Piezoelectric Transverse Coupling Factor, k31
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。