Corning Vycor® 7921 UV-Blocking Neodymium Blue Glass
Subcategory: Glass; Optical
Material Notes: Absorbs yellow and UV wavelengths through a process that introduces neodymium and cerium to the glass. Because the elements that create higher color temperature and UV blocking are a art of the glass structure, a lamp can be produced without substantial loss of visible light transmission as seen with coated bulbs. It can be run in high temperature lamp manufacturing processes without additional cost or process steps. Special Features: - Superior optical quality
- Tight dimensional control
- Thermal and chemical properties ideally suited to high temperatures.
- Excellent thermal shock resistance
Information provided by Corning Incorporated.
| Available Properties |
- Density
- CTE, linear 20°C
- Annealing Point
- Strain Point
- Transmission, Visible
- IR Transmittance
- UV Transmittance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|