EDO Ceramics EC-21 Barium Titanate Piezoelectric
Subcategory: Oxide, Other; Oxide, Titanium; Piezoelectric; Oxide
Key Words: BaTiO3; Barium Titanium Oxide
Material Notes: This modified barium titanate has been developed for operations at high power levels. It is characterized by its low impedance and low dielectric loss under high driving fields. This material is ideal for sonar and specialized transducers. Data provided by EDO Ceramics.
| Available Properties |
- Density
- Modulus of Elasticity
- Curie Temperature
- Dielectric Constant
- Dissipation Factor
- Piezoelectric Longitudinal Coupling Factor, k33
- Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V
- Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V
- Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N
- Piezoelectric Planar Coupling Factor, kp
- Piezoelectric Mechanical Q
- Piezoelectric Shear Coupling Factor, k15
- Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V
- Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N
- Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N
- Piezoelectric Transverse Coupling Factor, k31
- Thermal Conductivity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|