EDO Ceramics EC-57 Barium Titanate Piezoelectric
Subcategory: Oxide, Other; Oxide, Titanium; Piezoelectric; Oxide
Key Words: BaTiO3; Barium Titanium Oxide
Material Notes: This modified barium titanate has been developed to provide excellent stability of parameters from -40°C to 100C. This material has ideal characteristics for high power ultrasonic cleaning systems and low loss highly stable sonar projectors. Data provided by EDO Ceramics.
| Available Properties |
- Density
- Modulus of Elasticity
- Curie Temperature
- Dielectric Constant
- Dissipation Factor
- Piezoelectric Longitudinal Coupling Factor, k33
- Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V
- Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V
- Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N
- Piezoelectric Planar Coupling Factor, kp
- Piezoelectric Mechanical Q
- Piezoelectric Shear Coupling Factor, k15
- Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V
- Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N
- Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N
- Piezoelectric Transverse Coupling Factor, k31
- Thermal Conductivity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|