EDO Ceramics EC-64 Lead Zirconium Titanate Piezoelectric
Subcategory: Oxide, Zirconium; Oxide, Titanium; Piezoelectric; Oxide
Key Words: PZT; PbZrO3 - PbTiO3 Solid Solution
Material Notes: Developed for high power acoustic projectors. High coercive field, high coupling coefficient, low dielectric loss under high driving fields. Used for high power, low frequency broadband projectors and other high power electro-acoustic devices. Data provided by EDO Ceramics.
| Available Properties |
- Density
- Modulus of Elasticity
- Curie Temperature
- Dielectric Constant
- Dissipation Factor
- Piezoelectric Longitudinal Coupling Factor, k33
- Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V
- Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V
- Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N
- Piezoelectric Planar Coupling Factor, kp
- Piezoelectric Mechanical Q
- Piezoelectric Shear Coupling Factor, k15
- Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V
- Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N
- Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N
- Piezoelectric Transverse Coupling Factor, k31
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|