Ferro Aluminum Oxide P99
Subcategory: Oxide, Aluminum; Oxide
Key Words: Al2O3, alumina, aluminium oxide, aluminum oxide
Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.
| Available Properties |
- Density
- Water Absorption
- Open Porosity
- Weibull Modulus
- Knoop Microhardness
- Vickers Microhardness
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|