Ferro Binding Agents, Glazes & Sealants EG 2964
Subcategory: Glass
Material Notes: Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3
Ferro`s electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulating over glazes, binding agents and sealants for a variety of ceramic, metal, glass parts and substrates.Information provided by Ferro Corporation
| Available Properties |
- Density
- Particle Size
- CTE, linear 20°C
- CTE, linear 250°C
- Softening Point
- Annealing Point
- Transformation Temperature
- Processing Temperature
|
|
|
|