Ferro Dental Glasses EG 2738
Subcategory: Glass
Material Notes: Glass Type: Ba-Al-B-Si Typical Application: Glass Filler
Ferro`s Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also manufactures custom formulations to meet specific customer requirements. All powders are manufactured to tight composition, physical properties, and particle size distribution while maintaining low levels of heavy metal (Fe, Pb) contamination.Information provided by Ferro Corporation
| Available Properties |
- Density
- CTE, linear 250°C
- Softening Point
- Refractive Index
- Purity Levels
|
|
|
|