Ferro Passivation Glasses - High Voltage (Zn-B-Silicates) IX 2443
Subcategory: Glass; Oxide, Silicon; Oxide
Material Notes: Typical Powder Form: RWG, DSD
Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can be applied to wafers using thick film and electrophoresis methods. These products are formulated and produced to achieve low alkali and iron levels. These glasses are also used for encapsulation of rectifiers using glass beading application methods. IX 2443 is a crystallizing glass that when fired, closely matches the expansion of silicon for use on stacked-chip diodes for high voltage devices.Information provided by Ferro Corporation
| Available Properties |
- Density
- Particle Size
- Ionic Impurities - Na (Sodium)
- Ionic Impurities - K (Potassium)
- CTE, linear 20°C
- CTE, linear 250°C
- Crystallization Temperature
- Softening Point
- Transformation Temperature
- Processing Temperature
- Ionic Impurities - Li (Lithium) ppm, Max
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|