GE Quartz Type 214 Fused Quartz Tubing
Subcategory: Glass; Oxide, Silicon; Oxide
Close Analogs: GE Quartz became a part of Momentive Performance Materials in 2006.
Key Words: Quartz Tubes
Material Notes: Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halogen, and other quartz lamp applications. Softening point 1683°C. Annealing point 1215°C. Strain point 1120°C. Data provided by GE Quartz.
| Available Properties |
- Density
- Viscosity
- Knoop Microhardness
- Hardness, Mohs
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Modulus of Rupture
- Compressive Yield Strength
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Softening Point
- Annealing Point
- Strain Point
- Refractive Index
- Transmission, Visible
- IR Transmittance
- UV Transmittance
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|