AGY VeTron® Glass Fiber
Subcategory: Glass; Oxide, Silicon; Glass Fiber; Oxide; Composite Fibers
Material Notes: Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance. Information provided by AGY Holding Corp.
| Available Properties |
- Density
- Water Absorption
- Loss On Ignition
- Filament Diameter
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Maximum Service Temperature, Air
- Maximum Service Temperature, Inert
- Refractive Index
|
|
|
|
| Property Data |