Goodfellow Leachable Ceramic (Silica, Zircon, Alumina)
Subcategory: Oxide, Silicon
Material Notes: SiO2 50/ZrSiO4 40/Al2O3 10 General Description: This form of ceramic is used in the precision foundry industry. The tubes and rods are incorporated into moulds in the lost wax process. Using this technique, very fine tolerances on diameter can be obtained. The ceramic is leached away by the using sodium hydroxide solution once the metal has solidified. This leachable ceramic has a high porosity, does not have an organic binder, but does absorb water. Information provided by Goodfellow.
| Available Properties |
- Density
- Water Absorption at Saturation
- Porosity
- CTE, linear 20°C
- CTE, linear 1000°C
- Maximum Service Temperature, Air
- Chemical Resistance - Alkalis
- Chemical Resistance - Concentrated Acids
- Chemical Resistance - Dilute Acids
- Chemical Resistance - Halogens
- Chemical Resistance - Metals
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|