Gouda Vuurvast A 1 S Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.