Gouda Vuurvast AK 45 Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Segercone
- Thermal Shock Resistance
|
|
|
|