Gouda Vuurvast AK 46 S Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05% during the last 10 hours). Application: in anode baking furnaces. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Segercone
- Thermal Shock Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|