Gouda Vuurvast AK 60 A Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% between 14 and 24 hours at 1400°C at a load of 0.2 MPa). Application: incinerators, burner bricks, lime kilns, frit melting furnaces. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Segercone
- Thermal Shock Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|