Gouda Vuurvast AK 60 M Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: This quality is produced from high fired raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a maximum density is obtained. By firing at high temperatures and using mullite as a binder, a homogeneous brick is obtained with very good refractory properties. Application: checker bricks, supports for tunnel kiln cars, burner bricks. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Segercone
- Thermal Shock Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|