Gouda Vuurvast LP 85 AM Dense Refractory Brick
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron ladles, discharge zone of cement kilns. Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air