Gouda Vuurvast SiC 70 Dense Refractory Brick
Subcategory: Oxide, Silicon; Oxide
Material Notes: Description: This type of brick, based on silicon carbide, is because of a very good thermal shock resistance, abrasion resistance and a high thermal conductivity very well suited for waste incinerator furnaces, aluminum furnaces, muffle furnaces and applications where a high abrasive resistance is required Remarks: This data represents average values, obtained from samples that were cut from standard bricks. Information provided by Gouda Vuurvast.
| Available Properties |
- Density
- Porosity
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Thermal Shock Resistance
|
|
|
|