Gouda Vuurvast ADHESIET 170 P Dry Air-Setting Refractory Mortar
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: Adhesiet 170 P is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum melting and holding furnaces. Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. Only clean water should be added to make the mortar ready for use. Information provided by Gouda Vuurvast.
| Available Properties |
- Particle Size
- Maximum Service Temperature, Air
- Base Material
- Mixing Water
|
|
|
|
| Property Data |