Gouda Vuurvast ADHESIET 180 PCr Dry Air-Setting Refractory Mortar
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: Adhesiet 180 PCr is a Cr2O3 doped corundum mortar with a phosphate bond, supplied as a dry powder. This material is especially developed for high chemical resistance at very high temperatures. Remarks: Adhesiet mortars can be stored for an unlimited time if kept dry and cool. Only clean water should be added to make the mortar ready for use. Information provided by Gouda Vuurvast.