Gouda Vuurvast CURON 13 SC Dense Refractory Castable
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/holding furnaces and ladles. Due to its unique raw materials, Curon 13 S contains two hydraulic binders and therefore will remain very strong. Curon 13 SC is worldwide used in the aluminum and cement industry. Remarks: These values apply to cast products. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- ASTM Classification
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|