Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistance because of its low thermal expansion and allows a relatively high heating rate because of special additives. Remarks: These values apply to cast products. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- ASTM Classification
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|