Gouda Vuurvast CURON 140 K Dense Refractory Castable
Subcategory: Carbide; Oxide, Aluminum; Oxide
Material Notes: Description: This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strength over the whole range of temperatures. Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- ASTM Classification
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|
| Property Data |