Gouda Vuurvast CURON 165 Dense Refractory Castable
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage. Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- ASTM Classification
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|