Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements. Remarks: Indicated values apply to vibrated products. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|