Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be applied by casting or gunning. Warning: If the material is installed by gunning the values for cold crushing strength, thermal conductivity and bulk density after drying increase with ca. 15%. The material consumption increases with ca. 25%. Remarks: These values apply to cast products. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Particle Size
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- ASTM Classification
- Material Consumption per 1 m3
- Mixing Water
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|