Gouda Vuurvast CURAS 60 SD Moldable Refractory Material
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. This material is especially applicable in burner throats under severe conditions. Remarks: The stated chemical composition and physical properties represent average values. Information provided by Gouda Vuurvast.
| Available Properties |
- Bulk Density
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Bonding Type
- Material Consumption per 1 m3
- Mixing Water
- Segercone
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|