Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed with potable water to the required consistency. Curas 90 S PF is applied, for example, in FCC units. It can be installed very efficiently, instructions for use are available. Information provided by Gouda Vuurvast.