UCAR® Grade CBY Extruded Graphite
Subcategory: Graphite; Carbon
Material Notes: Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.Typical Applications: - Heat treating boats and trays
- Furnace parts
- Fused refractory molds
- Aluminum runout tables
- Induction furnace susceptors
- Refractory Systems applications such as blast furnace and submerged arc furnace linings
Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
| Available Properties |
- Density
- Particle Size
- Ash
- Flexural Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|