UCAR® Grade SF75 Extruded Graphite
Subcategory: Graphite; Carbon
Material Notes: Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
| Available Properties |
- Density
- Particle Size
- Ash
- Flexural Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|