UCAR® Grade PGW Pressure Molded Graphite
Subcategory: Graphite; Carbon
Material Notes: An economical low ash material with excellent thermal shock resistance, Grade PGW is well suited for the fine machining detail required in molds for casting metal shapes. Grade PGW is a molded version of Grade CBY with excellent internal structure.Typical Applications: - Pressure casting molds
- Centrifugal casting molds
- Large diameter susceptors, furnace bases and covers
- Heat shields
Tabular property data is typical across grain. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.