UCAR® Grade PGX Pressure Molded Graphite
Subcategory: Graphite; Carbon
Material Notes: Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications: - Fluidized bed reactors
- Centrifugal casting molds
- Large diameter molds and crucibles
- Monolithic composite tooling parts
- Induction and vacuum furnace parts
- Heat exchangers
- Chemical process equipment
Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
| Available Properties |
- Density
- Particle Size
- Ash
- Flexural Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|