H.C. Starck Zirconium Diboride Grade B, ZrB2
Subcategory: Boride
Material Notes:
- Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizing
- Crucible material for non-ferrous metals
- Ceramic shapes to be used in production of Al in Hall-Heroult cells
- Hot pressed TiB, armor plates
- Cutting tools and cermets, suitable for machining aluminum
- Metal Matrix Composites
- Antioxidant in carbon-bonded refractories
- Burnable absorbers for neutrons
|
|
|