H.C. Starck Aluminum Nitride AIN Grade B, AlN
Subcategory: Nitride
Material Notes:
- High thermally conductive ceramics
- Composite ceramics
- SiAlONs
- Heat sinks
- Electrically insulating packages for electronics
- Crucibles for metals and salt melts
- Thermally conductive filler for polymers
- Components in wafer processing (susceptors, chucks, carriers)
| Available Properties |
- Particle Size
- Specific Surface Area
|
|
|
|
| Property Data |