H.C. Starck Silicon Nitride Grade B7, Si3N4
Subcategory: Nitride
Material Notes: Alpha phase > 87%- Ceramic cutting tools
- Heavy duty components in automotive engines
- High performance parts for mechanical engineering
- Bearing components, like high precision balls
- SiAlONs
- Metallurgy (thermocouple protection tubes, stalk tubes, crucibles)
- Chemical engineering, e.g. heat exchangers
- Functional parts in textile machinery
- Releasing agent in Silicon ingot production
| Available Properties |
- Particle Size
- Specific Surface Area
|
|
|
|
| Property Data |