H.C. Starck Amperit® 704.072, Chromium Oxide (Cr2O3) 99.5%
Subcategory: Oxide, Other; Oxide
| Available Properties |
- Particle Size
- Acid Soluble wt%, max
|
|
|
|
| Property Data |