ICE Steatite L-5
Subcategory: Oxide, Magnesium; Oxide, Silicon; Oxide
Key Words: International Ceramic Engineering soapstone, talc, H2Mg3(SiO3)4
Material Notes: Data provided by the manufacturer, International Ceramic Engineering.
| Available Properties |
- Water Absorption
- Hardness, Mohs
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Yield Strength
- Dielectric Constant
- Dielectric Strength
- Dielectric Loss Index
- CTE, linear 500°C
- Maximum Service Temperature, Air
- Color
|
|
|
|
| Property Data |