Industrial Nanotech Nansulate™ - Translucent PT Insulation Coating

 

Subcategory: Ceramic/Metallic Coating

Material Notes:
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.

NANSULATE™ liquid applied insulation is a premium industrial grade rust proofing protective insulation coating containing Hydro-NM-Oxide, which is the best insulating material on the planet...by far. NANSULATE™, when fully cured, contains a high level of Hydro-NM-Oxide along with acrylic resin and performance additives. It has unique and astounding insulation properties which surpass all other forms of insulation previously available. Nansulate has proven resistance to both existing mold growth and new mold growth. Nansulate can also be used for Lead Abatement—as a lead encapsulation coating. 20 year warranty.

Uses: Pipes, Tanks, Trucks, Textile, Attics, Walls, Ships, Automotive, Containers, Residential, Commercial, Industrial

Corrosion protection and insulation are now combined into one, solving the costly problem of CUI (corrosion under insulation).
Excellent adhesion to a wide variety of substrates.
User-friendly with no special tools needed and easy to apply.
Effective three-coat system, which can be easily over-coated if desired.
Ability to see the substrate through the material allows for visual inspection of pipes, tank and equipment.
Mold resistance without use of potentially harmful anti-fungal agents
Encapsulate Lead with a smooth, water-based, environmentally friendly coating.

Information provided by Industrial Nanotech, Inc.

Available Properties
  • Density
  • Solids Content
  • Viscosity
  • Thickness
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Processing Temperature
  • Cure Time
  • Color
  • Coverage per gallon
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。