Kentucky-Tennessee Clay Company Jackson Ball Clay
Subcategory: Clay; Ball Clay
Key Words: Gleason, Tennessee, K-T clays, KT clays
Material Notes: A fine-grained, high alumina ball clay known for its excellent fired color, strength and plasticity. Used in both casting and plastic formed bodies.Applications: dinnerware, sanitaryware, artware, electrical porcelain, refractories, and emulsion applications. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.