Kentucky-Tennessee Clay Company Tennessee #5 Ball Clay
Subcategory: Clay; Ball Clay
Key Words: Gleason, ceramic castings, K-T clays, KT clays
Material Notes: An intermediate-grained, high organic ball clay with good strength, plasticity, and fast casting properties.Applications: sanitaryware, dinnerware, artware, refractory casting applications, and plastic formed bodies. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.