Kentucky-Tennessee Clay Company Tennessee #10 Ball Clay
Subcategory: Clay; Ball Clay
Key Words: Gleason, K-T clays, KT clays
Material Notes: A low organic, medium-grained, low residue ball clay with unparalleled white-firing characteristics due to its high kaolintic content.Applications: refractory and fast-firing applications. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
- Specific Surface Area
|
|
|
|