Kentucky-Tennessee Clay Company MB Ball Clay
Subcategory: Clay; Ball Clay
Key Words: Mayfield, Kentucky ball clays, MB, K-T clays, KT clays
Material Notes: An excellent white firing ball clay that can be used to improve the fired color in ceramic applications. Also used to provide increased viscosity and suspension properties to coal tar and asphalt emulsions. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
- Specific Surface Area
|
|
|
|
| Property Data |