Kentucky-Tennessee Clay Company Kentucky Stone Ball Clay
Subcategory: Clay; Ball Clay
Key Words: Mayfield, Kentucky ball clays, Kentucky Stone, K-T clays, KT clays
Material Notes: A coarse-grained, siliceous, illitic ball clay known for its high strength and plasticity.Applications: artware and ceramic tiles. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
- Specific Surface Area
|
|
|
|