Kentucky-Tennessee Clay Company Kingsley-Rogers Ceramic Grade Kaolin
Subcategory: Clay; Kaolin
Key Words: Sandersville, Georgia Ceramic kaolins, Kingsley-Rogers, K-T clays, KT clays
Material Notes: An intermediate-grained kaolin.Applications: ceramic casting and pressing applications, dinnerware, tile, artware and electrical porcelain. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
|
|
|
|
| Property Data |