Kentucky-Tennessee Clay Company LGB-1 Hard Clay, Kaolin Filler Extender
Subcategory: Clay; Kaolin; Filler Extender
Key Words: K-T clays, KT clays
Material Notes: This hard clay product is a naturally occurring kaolin that is processed by air-floatation. It is routinely used where economical processing and compound reinforcement are needed. Air-floated clays are the most widely used and the least expensive functional fillers employed in the elastomeric industry. GE brightness: 70 - 80 Moisture Content: 1.0% max +325 Mesh: 0.10 max Applications: soft and hard rubber compounds, plastics, adhesives, protective coatings, traffic paints, joint compounds, agricultural fillers. Information provided by the manufacturer, Kentucky-Tennessee Clay Company.
| Available Properties |
- Specific Surface Area
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|