Concrete, clinker aggregate
Subcategory: Concrete
Key Words: lightweight aggregates
Material Notes: 0.04-0.08% drying shrinkage. Consists only of well-burnt furnace residues which have been fused or sintered into lumps.
| Available Properties |
- Density
- Compressive Yield Strength
- Thermal Conductivity
|
|
|
|
| Property Data |