Concrete, foamed blastfurnace slag aggregate
Subcategory: Concrete
Key Words: lightweight aggregates
Material Notes: 0.03-0.07% drying shrinkage. Manufactured by treating molten blastfurnace slag with sufficient water or other suitable medium to produce a cellular dry product which is crushed and graded as required.
| Available Properties |
- Density
- Compressive Yield Strength
- Thermal Conductivity
|
|
|
|
| Property Data |