Concrete, pumice aggregate
Subcategory: Concrete
Key Words: lightweight aggregates
Material Notes: 0.04-0.08% drying shrinkage. A spongy lava which, in its natural state needs only to be crushed, washed, to remove dust and clay, and graded.