Glass Fiber Reinforced Concrete
Subcategory: Concrete
Material Notes: Property values are for samples after 28 days. Glass fiber reinforcement significantly increases the flexural strength of concrete. The fiber reinforcement also leads to a somewhat gradual failure, rather than a sudden failure.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Impact
|
|
|
|